Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

how it can be traced that SS electrode is used instead of 9% Ni

Status
Not open for further replies.

Ironmanmech

Mechanical
Joined
Jun 22, 2013
Messages
2

Dear members,

I wonder if anyone could help me out with the following matter:

how it can be traced that SS electrode is used rather than 9% Ni in order to weld the 9% Ni plates of LNG Tanks (without excavation or any types of destructing welded areas) mostly when it has been used at the first pass or second.


your help is quite appreciated
 
If the area in question is accessible, an X-Ray fluorescence material identifier could show what the chemical composition of the finished weld is.
 
Hi again,

Thank you dear fegenbush for your answer.
The area in question is accessible, but, the instrument you mentioned identifies the material and filler metal percentage of surface passes. we need to identify the material composition of first passes of a Double-V weld joint.

Great thanks
 