Hello Everyone!

I have been trying to develop a product which requires the assembly of a silicone slit valve in a plastic component.
I bought a product containing this assembly but I can't seem to figure out how it is done.
The picture below show what I am trying to achieve.

IMAG0118_ruoc1r.jpg


I am assuming that the same principal is applied to achieve the assembly in this picture:

IMAG0119_lv5thc.jpg


Any advice would be helpful!

Thanks
Abhinav
 
My first guess is that since the transparent component is injection molded, then the total assembly would be done in a co-injection process. This would support high-volume requirements.

Another guess is a 2-part assembly with the silicone component over-molded/insert-molded into the full assembly, or assembled and heat-staked or ultrasonically welded to the transparent component.

TygerDawg
Blue Technik LLC
Virtuoso Robotics Engineering
 
UV-cured adhesives could also play a role.

"Art without engineering is dreaming; Engineering without art is calculating."

Have you read faq731-376 to make the best use of these Forums?
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top