I'm assuming shear strength relates to tensile strength by 0.6 Fu. Is this correct, if so where does it come from?

 
Replies continue below

Recommended for you

Physics.

If you want data showing this, look at MIL-HDBK-5 or the ASM Handbooks.

MIL-HDBK-5, Revision J is here:


ASM Handbook Volumes 1 & 2 have what you want for many alloys, available here:


Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
If you look hard enough you will find that for various classes of alloys the value may be slightly higher or lower than 0.6
It depends on some issues related the structure of the alloy.

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps