Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

How Does Concrete Sampling for Cubes/Cylinders and Slump Happen in Your Neck of the Woods

Status
Not open for further replies.

BigH

Geotechnical
Joined
Dec 1, 2002
Messages
6,012
Location
TJ
Just interested to see what kind of response we can get on the issue of proper concrete sampling.

As ASTM and BS EN (though in a round about way) say to sample, even for spot samples, to let the first part (0.3 to 0.5 m3) go, then commence spot or preferably composite samples, I have found on my Asian jobs, it is very difficult to get the concrete QC group to do this - they usually take the sample as the transit mixer arrives on site before any concrete "goes".

So what is done in your neck of the woods?
 
No takers, eh. Just trying to see how far off spec various areas go in sampling.
 