Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

How do you estimate the amount of welding electrode/wire for a job? 1

Status
Not open for further replies.

DrDarrell

Mechanical
Apr 25, 2001
22
Is there a rule of thumb for estimating the amount of welding wire or welding electrode that is needed for any specific job?

For example: If I have a 1/2" fillet weld 20" long, how much welding electrode do I need to buy to complete the job?

I would like a rule of thumb for both shielded arc and tig.

Is there a difference in the estimate for different materials?

Thank you in advance for your help.

Darrell
 
Replies continue below

Recommended for you

Basically it is the volume of the weld multipled by the density of the material.

for SMAW, stick welding multiple this value by 1.3 to 1.4 to account for stub losses.

for GTAW (TIG) welding use a factor of 1.1 (10% extra)

1/2" fillet 20" long

((1/2inch*0.707)^2)*20inch*1.3 *490lb/ft3*1ft3/1728 in3=
-------------------
2

= 0.35 lbs (SMAW 1/2" fillet @ 20")


Hope this helps, Rich
 