There is a product analysis tol for nearly all elements in metal alloys.
The Heat Analysis has to meet the specification ranges, but the product analysis has an additional allowance.
There is also the fact that they may be making a grade for someone with higher Mn that is not ASME (perhaps SAE or proprietary).
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed