I have been investigating Charpy test failures in our steel foundry recently and am evaluating our process. One item of concern is a change that was made a couple years ago to our hot topping. Can someone suggest a test that can be done to validate that the hot topping is still working properly? I have put out a call to the supplier, but haven't heard anything yet.

Thank you for your suggestions.
 
Solidification/cooling rate and depth of shrinkage are the first things that come to mind.
We used to measure both when we were making changes in molds or topping.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 