I have a 250PFC hot rolled channel member that is cast into a large reinforced concrete (RC) wall . Thus a fixed member with a point load at the end. Does anyone know how to calculate the development length of the section into the rc wall?
thanks in advance

________________________________
Use RAPT for Slender RC Columns
 
Replies continue below

Recommended for you

Development length for what - tension or bending?

If it is just tension then look up the values for plain bar and backcalculate the bond stress then apply this across the rectangular perimeter of the section (i.e. twice the width plus twice the height) which should definately be conservative.

If for bending then you also need to take bearing stress into account.
 
thanks csd72..very helpful ---its for tension under bending

________________________________
Use RAPT for Slender RC Columns
 
If it is just bending then treat it as a pure horizontal bearing stress problem like a pile embedded in rock. The allowable bearing stress in the concrete will dictate.

Look up a good precast concrete book and you will find a section on column pockets that will give you just what you need.
 
I would provide and end plate to the PFC and either weld a cogged bar or shear stud to anchor the PFC to the concrete.
 