Guys,
we are having a little debate in work with relation to weld positions. The attached doc shows the weld prep, which is a two sided butt weld, which is back-gouged after first few passes. The weld is approx 6 feet off the ground. we reckon the position is horizontal, our client reckons it is overhead. The client is not being awkward, and we have a procedure which will cover us anyway, but would like some other opinions anyway
regards & thanks
Declan
we are having a little debate in work with relation to weld positions. The attached doc shows the weld prep, which is a two sided butt weld, which is back-gouged after first few passes. The weld is approx 6 feet off the ground. we reckon the position is horizontal, our client reckons it is overhead. The client is not being awkward, and we have a procedure which will cover us anyway, but would like some other opinions anyway
regards & thanks
Declan