sir
We need a clarification regarding the hoop stress and deformation of thin cylinder after mounting a wire over the cylinder surface with the following data.
Tension in the mounting wire = 6 kg.
Cross-section of wire = 2x0.5mm(height & width)
Wire material = steel
Length of the cylinder = 1000 mm
O.D of the cylinder = 1200 mm
Thickness of the cylinder = 20 mm
Cylinder Material = Cast Iron (youngs modulus = 1E5 N/sq.mm,
Poission ratio = 0.23)
After completing various operations the roundness and straightness of the cyl. are within the limits.(less than 0.1mm).
But we are getting a variatoin of 0.1 to 0.15 mm over the cylinder surface after wire mounting. Sir please specify whether the problem is due to hoop stress or other factors like atm. temp. 35-40 degrees celsius , Casting .
Kindly send us your comments at the earliest.
Thanking you
With regards
K.Soundararajan
L.M.W Ltd
Coimbatore-641020
India
E-Mail: lmwrd@md3.vsnl.net.in