hcoles
Mechanical
- Sep 12, 2006
- 16
Would like some help finding link to equations to calculate the hoop stresses in the female side of NPTF/NPTF 1 1/4" connection. The material is brass. The current best guide from Parker is to use the TFFT. ... for 1 1/4" the TFFT is 1 1/2 turns to 2 1/2 turns. Some fittings may have been over torqued, i.e. the TFFT was not followed. How can I get an idea how much stress was put into the fittings before they failed? The failure was a straight crack running along the outside of the female fitting parallel to the flow direction. I think there should be some idea how much hoop stress is in a brass fitting when assembled e.g. 2 turns from finger tight (TFFT). I'm looking for that type of equation.