Hole for Nozzle thru a Category A Joint

Status
Not open for further replies.

DLind2005

Mechanical
Feb 24, 2014
9
I am in a jam with a vendor who processed the holes in an ERW SA-53-B Pipe and put a hole in the weld seam. What requirements do I need to do to make sure the shell is usable and the weld seam has not been affected? Do I need to perform RT work on the seam? Is the hole through the Category A joint ok? What makes it ok? Any help or insight would help me greatly!

Thanks!
 
Replies continue below

Recommended for you

If you're just concerned from a Code standpoint review UW 14. Customer restrictions may be tighter.
 
I see no problems, there are no prohibitions in opening on a weld seam of ERW pipe.
 