Hi,

Does anyone have any information on the dimensions and properties of a No 312 Fabric Mesh. I have looked at the CIA Concrete 2017 Historical Reinforcement paper and the reinforcements shown are for only 601 to 610 and I am unable to find the A84-1958 Standard.

This reinforcement mesh has been called up on a drawing from 1970/1971.

Regards,
Nick
 
Replies continue below

Recommended for you

Assuming this is an Australian reinforcing type, ARC Reo manufacture WeldMesh in a type configuration “WG312” which is 3.15 mm dia galvanized wires with 25mm x 50 mm wire spacing.

Seems to be more of a fencing or shelving product than concrete reinforcing.

Link

Not sure if this makes any sense for your situation, if not, try the Concrete Institute of Australia - they may be able to assist.
 