They are very low values, but in the absence of better information, you might consider using the default values of Chapter 7 of FEMA 356. They are 300 psi for poor condition, 600 psi for fair condition, and 900 psi for good condition. These are said to be lower bound values, and you can multiply these by a factor of 1.3 to arrive at the expected strength value for each respective condition.