jerseyshore - same thing around here. But to that I say too bad. I work primarily for Architects, not contractors. So if a contractor says "hey, I want to epoxy it in" I tell them no. If they say they already did it, I tell them to provide me with a design saying it is equal to or exceeds the capacity of what I had designed for my approval. I also tell them that if they hit/cut through any rebar, they'll probably have to chip out the concrete, repair the rebar, and recast it, though that depends on what it is and how critical it is. And once you really start looking at the installation procedures for those...they don't work very well if you have any rebar in the vicinity. And the edge distance almost never works in foundation walls with slabs on grade.