I am putting a kwik bolt 3 near an old construction joint in 4000 p.s.i. concrete. Is there any documentation that provides guidance on the subject. It will not land on the old joint. The joint is tapered into a curve formed into the wall. I am putting an anchor about 2-3" away from the joint. The joint is about 1" wide and a curved v about 1" deep.
Anyone have documentation or experience on this issue or comments.
Thanks
Anyone have documentation or experience on this issue or comments.