Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations Ron247 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Hight Strength Flange Bolts

Status
Not open for further replies.

engpes

Mechanical
Feb 10, 2010
175
I have an ASME VIII low temperature / low pressure applications (275 psig @ 140 F). I have a custom flange design and the number of bolts and size is critical.

I am currently using 1/2" 193-B7 studs and am asking if their is any other ASME acceptable stud material with a higher strength (yield and tensile).

Thank you in advance for your help. This is something I would need in the very near future for this one-time application.

 
Replies continue below

Recommended for you

engpes, there are a number of stronger bolt materials permitted for Sec VIII, Div 1, Div 2, both ferrous and non-.

Do you have access to Sec II, Part D by chance? If so, see Table 3. You really need to select based on your service, any limitations noted in Table 3 and commercial considerations.

I have used SA-354 BD (150 ksi min tensile) once before.

Regards,

Mike
 
Go over section 8 Div 1, App. 2, which concerns flange design and goes over adequate bolt load for sealing.

At 275 psi, generally B7 bolts are suitable for a variety of flange and gasket combinations, especially for class 300 and above flanges, so I would look into off the shelf components to suit your needs.
 
ASTM A193-B7 Studs are not permitted under CSA Z245.15 as low thermal application flange bolting.

You should be using a Category II Standard fastener (i.e. Sweet application - Cold Temperature), something like ASTM A320 L7 Stud with ASTM A194 4/7-S4 Heavy Hex Nut.

The Category II NACE fastener is ASTM A320-L7M with ASTM A194 7M-S4 Heavy Hex Nut. You could theoretically use this low temperature NACE faster(s) for a low temperature standard application, BUT NOT the reverse.

Be careful with fastener selection, your initial choice is only good for a Standard Service Category I application, which is not low temperature. B7 studs are not Notch Toughness and therefore, restricted for use under the spirit of the code.

Kenneth J Hueston, PEng
Principal
Sturni-Hueston Engineering Inc
Edmonton, Alberta Canada
 
The following materials are in the ASME B&PV Code and have allowable stress higher than B7:

XM-19 (austenitic Fe-Cr-Ni-Mn alloy)
17-4 PH (martensitic Fe-Cr-Ni-Cu alloy)
B22 (4140 steel)
718 (nickel alloy)
SA 574 (4140 steel)
 