Will ACM withstand 230°C for 24 hours?
 
Depends on the environment, but it should be ok away from moisture/acids/bases.
see
edit - whoops, you said C not F. Dunno, probably not that hot, very few plastics can survive above 400F/200C and acrylics aren't from the family of polymers (-imides, arylates, fluorocarbons) that can survive high heat.
 
For this time and temperature ACM cn resist, but a selection of high performance antioxidant is very importante, as the curing system used, too
 