1
I am attempting to take a thermographic image of a flat plate burner from above, and this requires that I use a 45 degree mirror to redirect the radiation. At the maximum output of the burner, I have recorded a temperature of approximately 95 C where the mirror needs to be placed.

I am having trouble sourcing a mirror that will provide sufficient IR radiation reflection and be able to withstand the higher temperatures.

Does anyone have any idea where I could find such a mirror?

Thanks.

 
Replies continue below

Recommended for you

"sufficient IR radiation reflection" ???

The source must be quite hot; there should be plenty of photons, even if the reflectivity is degraded. What reflectively requirement are you specifying?

TTFN
faq731-376
7ofakss
 
For thermal imaging, you probably need a "first surface" mirror.
Googling high-temperatre first-surface mirror lead to this:
They give the reflectivity for 400-800nm. If your camera operates at longer wavelength, you'd have to ask them for characteristics in that range (or search another)

=====================================
(2B)+(2B)' ?
 