I am working on a project that involves a short section of piping that is at 1,800°F and 5 psig design conditions. I have been requested to provide the stress analysis. They want the design to B31.3, even though it is not considered pressure pipe. The conundrum is what allowable stresses to use as B31.3 only goes to 1,500°F and the stress is only 1,100 psi. The material they plan to use is A316-Type 321H. I have a similar question for the flanges (B16.5 allows 1,500°F @ 40 psi).
I know that B31.3 considers high pressure design but what is your experience with high temperature piping? Any suggestions as to how to approach this from a pipe stresser point of view?
Thank you in advance!
I know that B31.3 considers high pressure design but what is your experience with high temperature piping? Any suggestions as to how to approach this from a pipe stresser point of view?