I am working on a preliminary design of a pressure vessel with design paramaters of 100 psi and 1600F. Once I get something that seems workable then I will turn it over to a Code shop to have them run the ASME Sect. 8 Div. 1 calcs on it.
I am looking at Nickel based super alloys for corrosion resistiance in Sect. 2 Table 1b, specifically UNS N06230. This alloy has note G5 which pertains to creep and note T16 which deals with time-dependent properties. I have also heard that there are allowances for analyzing flanges at temperatures lower than what is stamped as long as the U1 papers detail it and the flange is controlled at the lower temp.
Three questions:
1) How is creep analysed in the code?
2) What is the significance of time-dependent properties?
3) Is there a procedure for derating flanges in the code as mentioned above?
Thank you for your time in reviewing my application.
I am looking at Nickel based super alloys for corrosion resistiance in Sect. 2 Table 1b, specifically UNS N06230. This alloy has note G5 which pertains to creep and note T16 which deals with time-dependent properties. I have also heard that there are allowances for analyzing flanges at temperatures lower than what is stamped as long as the U1 papers detail it and the flange is controlled at the lower temp.
Three questions:
1) How is creep analysed in the code?
2) What is the significance of time-dependent properties?
3) Is there a procedure for derating flanges in the code as mentioned above?