I am trying to determine the allowable fatigue stress amplitude limits for thermowells at temperatures above those listed in the design fatigue curves. I am working with the ASME standard PTC 19.3 TW 2010, which has the fatigue stress amplitude limits listed for various materials, and which were determined in accordance with Section VIII Div 2. But since the fatigue curves in VIII-2 are limited to 800°F, I am not sure how to proceed for the higher temperatures.
The stress limits I am looking at seem to be far below the creep stress data (1% per 10000hrs) I have been able to find.