Oct 29, 2001 #1 langahl Mechanical Joined Aug 8, 2001 Messages 11 Location US I need to differentiate between 'Hatelloy C' and 'Hastelloy C'. Would appreciate all the assistance I can get. Thanks. langahl@netscape.net
I need to differentiate between 'Hatelloy C' and 'Hastelloy C'. Would appreciate all the assistance I can get. Thanks. langahl@netscape.net
Nov 13, 2001 #2 mikemkc Mechanical Joined Nov 12, 2001 Messages 12 Location US Sir, You have fallen victim to a typo. "Woldman's Engineering Alloys" has no listing for Hatealloy C, nor have I seen or heard of such a material in 25 years of PV design. Upvote 0 Downvote
Sir, You have fallen victim to a typo. "Woldman's Engineering Alloys" has no listing for Hatealloy C, nor have I seen or heard of such a material in 25 years of PV design.