I need to differentiate between 'Hatelloy C' and 'Hastelloy C'. Would appreciate all the assistance I can get.

Thanks.
langahl@netscape.net
 
Replies continue below

Recommended for you

Sir,

You have fallen victim to a typo. "Woldman's Engineering Alloys" has no listing for Hatealloy C, nor have I seen or heard of such a material in 25 years of PV design.
 