Feb 29, 2008 #1 TWR2 Mining Joined Jan 16, 2008 Messages 12 Location US Good Morning: I am looking for High temp stainless alloy for use in a reducing envirnment, operating temperatures of 2550 F. Looking for cast specification. Regards, TWR
Good Morning: I am looking for High temp stainless alloy for use in a reducing envirnment, operating temperatures of 2550 F. Looking for cast specification. Regards, TWR
Feb 29, 2008 #2 stanweld Materials Joined May 9, 2003 Messages 2,906 Location US A stainless steel does not exist for your application. Ceramics or refractory materials would need to be employed. Upvote 0 Downvote
A stainless steel does not exist for your application. Ceramics or refractory materials would need to be employed.
Feb 29, 2008 #3 EdStainless Materials Joined May 20, 2004 Messages 16,364 Location Waukesha WI USA There are a number of high temp cast Ni alloys that you can use at 2100F or a little higher. Leek on the web site of Wisconsin Centrifugal (Metaltek) to get an idea of what some of these are. = = = = = = = = = = = = = = = = = = = = Plymouth Tube Upvote 0 Downvote
There are a number of high temp cast Ni alloys that you can use at 2100F or a little higher. Leek on the web site of Wisconsin Centrifugal (Metaltek) to get an idea of what some of these are. = = = = = = = = = = = = = = = = = = = = Plymouth Tube