Good Morning:

I am looking for High temp stainless alloy for use in a reducing envirnment, operating temperatures of 2550 F. Looking for cast specification.

Regards,

TWR
 
Replies continue below

Recommended for you

A stainless steel does not exist for your application. Ceramics or refractory materials would need to be employed.

 
There are a number of high temp cast Ni alloys that you can use at 2100F or a little higher.
Leek on the web site of Wisconsin Centrifugal (Metaltek) to get an idea of what some of these are.

= = = = = = = = = = = = = = = = = = = =