Hi!

I've been researching various polymers for a temp range or -40F to 250F, that need to be resistant to 242 oil and 80W90 oil.

I've found PEEK as an option, but was hoping to find some less expensive options.

Thanks much for your input!
 
Replies continue below

Recommended for you

Polyphenyl sulfone is very resistance to car engine oil at operating temperature. I remember Stratasys made a prototype oil filter from that and ran it on a car for quite some time.

Chris DeArmitt PhD FRSC CChem
 
Nylon 6.6 is probably OK. If the load is high, nylon 4.6 will be better and you will have a whole truckload of change compared to buying PEEK.

Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
Are there mechanical property requirements? PTFE and various fluoroelastomers are used in these types of applications. For strong and stiff, consider polyamides, PPS, and PEEK.

80W90 is a lubricant used for gear applications such as hypoids for automotive axles. Yes, they can contain sulfur additives to provide EP (extreme pressure) performance.
 
Nylons are OK with gear oils. I don't know what 242 oil is, but unless it contains something like phenol or it is acidic, it won't touch nylons


Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
Sorry....typo...It's 424 oil is hydraulic oil.

Thank you for all of the responses.
 
phenolics, different grades are available depending on strength requirements, injection moldedable, cheap <$2/lb, love any hydrocarbon
 