Hello,
Can someone give to me informations about reactions on 316L SS into high temp. 200'C ~ 300'C. What can happened if I will take two SS parts,screw them together and increase temp?
Can they stuck together?

Thanks in advance for answer
Patkop
 
In the temperature range of 200-300Celsius in nomal atmosphere,nothing is going to happen to 316L screws..

Save water Drink Beer
 
There is a strong tendency for the threads of stainless nuts and bolts to gall, especially when the nut and the bolt are the same alloy. Even worse at high temps.
 