High temp. and Stainless Steel

Status
Not open for further replies.

PatKop

Industrial
Sep 18, 2007
4
Hello,
Can someone give to me informations about reactions on 316L SS into high temp. 200'C ~ 300'C. What can happened if I will take two SS parts,screw them together and increase temp?
Can they stuck together?

Thanks in advance for answer
Patkop
 
Replies continue below

Recommended for you

In the temperature range of 200-300Celsius in nomal atmosphere,nothing is going to happen to 316L screws..

Save water Drink Beer
 
There is a strong tendency for the threads of stainless nuts and bolts to gall, especially when the nut and the bolt are the same alloy. Even worse at high temps.
 