Hello, I am working on a precast bridge where there is continuity provided across the slab. I am checking the stress at top of the slab as part of service limit check. I noticed at the supports I am exceeding the 0.19sqrtf'c. I have been thinking of possible solutions such as jacking the prestress at both ends of the beam so it might lower the demand on the slab. However I wonder if any one experienced something like it before on how to address stresses exceeding the tensile limit at the supports.