I need strong clear glass that can withstand 150 kilo Newton per meter squared (or 22 psi). Limited by the weight 270 kg per meter square (or 55.4 lbs/ft2). Open to suggestion.

Glass must be 4,100 X 2,700 mm.
 
Replies continue below

Recommended for you

What is the application?
Are there any limitations on thickness or optics?

"On the human scale, the laws of Newtonian Physics are non-negotiable"
 
Chemically strengthened soda lime glass or alumino silicate glass can have a failure strength in the range of 40-120ksi depending on the processing. That is a tensile strength, not a surface load. If you have a load normal to the plane of the glass of 22psi, then its a different story. There is a chem tank I know of which is 5m long. Knowing the application would help.
 