Can anyone suggest a supplier for either M1 or M2 high speed steel filler rod? A Google search surprisingly did not result in any welding supply houses that seem to carry these products. Thanks.


Maui

 
Thanks Metengr. Unfortunately, they don't carry it either. But they did direct me to a company that does - High Quality Alloys located at
Maui
 
Try these two they should have something up 3/4" dia.

I was trying to look through my notes I don’t see in particular, but Hastalloy C is a good choice on a several tool steels. The trick is in the preheat and maintaining the interpass temperature.


 