High Pressure Sodium Hyperchlorite injection

Status
Not open for further replies.

misco41

Civil/Environmental
Joined
Nov 26, 2004
Messages
2
Location
GB
Can anyone advise ?

I have a situation where I need to dose sodium hyperchlorite into a trunk main supply with operating pressures in the range 18 - 22bar.

This resticts me from using a standard PVC lance as these are only rated to 16bar. I have been told that a titanium lance would be suitable as this would accommodate the high pressures and is resilient to Cl.

Would this be the solution ? Any guidance would be appreciated.

 
Do a lookup for "injection quill" on the web. You will find many companies with many different quills. Saftflo is one of those companies with various injection assemblies/parts.

You can get them in PVC, Polypropylene, S.S., Hastelloy, etc. The S.S. and Hastelloy will hit pressure ranges higher than what you are talking and they should handle the CL.
 
Misco 41

Hypo will eat the stainless steel (any grade) injection lance/ Quill

But Hastelloy C as I remember is good for chlorine gas and Sodium Hypochlorite.

Hope this helps
 
semo / Tonka73,

Many thanks for your reply. I have been advised that Hastelloy is extemely difficult to machine, and work hardens terribly ? Any commnets...

 
You could probably find a made-up lance. Try Nalco
 