I have received a valve casting per ASTM A351-2003 grade CD4MCu. I performed Positive Identfication Inspection (PMI) and found all the elements meets the ASTM specification with exception of Mn%. Instead of max 1% Mn material that I received has Mn 1.5 % - 2%. Manganise should improve the mechanical strength of the cating but, I am not sure if it will effect the chemical resistance of the material or the macro structure of the material.
As a note: forged grade F51 has 2% Mn.