I am searching for a high heat over 1200 degrees, nonmagnetic, conductive material to be placed in an induction heater between the coil and the part.
 
Replies continue below

Recommended for you

If F, then, depending on mechanical duty, a stabilised austenitic like 321 or 347 springs to mind. it's non-magnetic as long as it's not cold worked. (Note that this temperature will sensitize an unstabilized grade. Depending on your environment, it might well then corrode.) However, it's not a brilliant electrical conductor. Depends how good a conductor you need it to be.

If temp is C, you're into some relatively exotic stuff beyond my ken.

 
If conductive, it will heat up,too !

<nbucska@pcperipherals.com>
 