Dear group,
I have steel grade with following composition:
%c=0.13
%Mn=0.60
%Ni=4.9
%Ti=0.60
%Si=0.50
%Cr=21.0
%S=0.01
what is reason for adding Ti to this steel grade?
Best Regards