Dear group,
I have steel grade with following composition:
%c=0.13
%Mn=0.60
%Ni=4.9
%Ti=0.60
%Si=0.50
%Cr=21.0
%S=0.01

what is reason for adding Ti to this steel grade?
Best Regards
 
Based on the Cr/Ni contents, your stated composition looks more like a fit with a duplex stainless steel casting. Do you have the specification for this alloy? Deliberate additions of Ti can serve several functions in alloys, as a deoxidizer, or as a strengthener for precipitation hardening capability and/or stabilizer to form TiC instead of harmful chromium carbides.

Can you provide more information as to your use of this alloy?
 
Internal combustion engine exhaust valves sometimes are made with 21-4 steel.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Chemical composition is for 12Ch21N5T steel grade(GOST 5632).Unfortunately I have not GOST standard.
 
this looks a lot like SAF 2205 without the Mo and the N but with higher C
 