Hello all,
I have come across a statement regarding HIC in a material selection report for CO2/H2S wet sour service application. The statement reads 'equipment operating above 60 degC is not prone to HIC'. Is this indeed correct? If so, can anyone provide a technical reasoning?
Many thanks,
midris
I have come across a statement regarding HIC in a material selection report for CO2/H2S wet sour service application. The statement reads 'equipment operating above 60 degC is not prone to HIC'. Is this indeed correct? If so, can anyone provide a technical reasoning?
Many thanks,
midris