Hi all,
I am in the process of evaluating bids for pipes to be used in a sour service. NACE MR 0175 is applicable for these pipes.
Majority of vendors are stating that since they are supplying pipes with sulpur content less thant 0.01%, HIC test need not be done. Is this an acceptable condition?
Can anyone here shed some light on the actual requirement of HIC and SSC testing on pipes used for severe sour service as per NACE standard?
Pipe Material: API 5LB PSL-2.
Many thanks
I am in the process of evaluating bids for pipes to be used in a sour service. NACE MR 0175 is applicable for these pipes.
Majority of vendors are stating that since they are supplying pipes with sulpur content less thant 0.01%, HIC test need not be done. Is this an acceptable condition?
Can anyone here shed some light on the actual requirement of HIC and SSC testing on pipes used for severe sour service as per NACE standard?
Pipe Material: API 5LB PSL-2.
Many thanks