Hello Friends,
We are working on NACE materials recently. I have a question about HIC the SSC test. Normally according to NACE MR0175, materials with controlled hardness, content of S and P, and yield strength according to MR0175 is acceptable for NACE application. Sometimes customer need HIC and SSC test, sometimes no need.
My question is under what condition we should request HIC test and SSC test, at same time under what condition just request NACE application only.
 
Replies continue below

Recommended for you

If the material complies with all other requirements, it is either at the discretion of the end user or as directed by another applicable standard, e.g. ISO 3183 for linepipe.

Steve Jones
Materials & Corrosion Engineer
 
You need to do the test when the material isn't pre-qualified into MR0175 or if the environnement is more severe as authorized.
 