A client mentioned Hibble Blocks but I've never heard of them. Anyone have an explanation? Where can I get more info?
 
Replies continue below

Recommended for you

I feel as though I should say something like "The hawk flies at midnight".

I take it you don't know then? Or did I fall for one of those builders jokes?
 
Sorry,
I'm at the ragged end of a long week (is it only Wednesday). I don't know what the Hibble blocks are. I just thought of "Weebles Wobble .....".
 
Are you sure he did not mean Hebel Blocks. If so it is a precast autoclaved aerated concrete block. For information go to
 
Thanks, it must be hebel. I was able to get the hebel.com to work and printed out a bunch of info. Thanks everyone (except Kramer who had me thinking I was at the bad end of a builder's joke).
 