Hi.
I am searching for the manufacturer of a Carbon Epoxy prepreg with T300 and N5208. Does anybody knows?!
Thanks in advance!
 
Yes, I can try to contact all the companies but the problem is that I don't even know if it is a standard prepreg. What I am searching for is the prepreg properties including the thickness manufactured, since I need to make an isotropic laminate of 0.5 mm with a minimum of 6 layers. That is why I need to know where this prepreg is available. In the web pages you sent, it is possible that on there is a company that produces it, but still it will take a lot of time to find out!
Thanks anyway!
 
probably a bit late now but I buy lots of T300 T700 etc c/f epoxy prepreg. IT TorayCo fabric with the prepreggers resins system.
What is the N5208? and why that resin system? I think it may be Newport Resins system
 
I found somewhere the properties of this prepreg and they were the most suitable for me. This epoxy resin was increasing the stiffness of the ply.
Later, I decided to propose a different material which can be also useful, the Carbon/Cyanate M-40J / 954-6 from Hexcel, so I stopped my search for the other.
Thanks anyway.
 