scarecrow55
Mechanical
I have a hi strength bolt (12.9) going into a cast steel body - (no I can't change it), if I work out the engagement length based on the relative UTS of the materials I get a factor of 2.4 x the engagement length of the correct "nut" so I can tighten it right up.
All well & good but surely there must be a limit, infact 2.4 seems a bit excessive - If you use the UTS for wood you'ed get an engagement length of a few feet but I bet it wouldn't work.
Anyone know the limits? could I work on say the forces on the first 5 thrds or so?
Thanks
All well & good but surely there must be a limit, infact 2.4 seems a bit excessive - If you use the UTS for wood you'ed get an engagement length of a few feet but I bet it wouldn't work.
Anyone know the limits? could I work on say the forces on the first 5 thrds or so?
Thanks