Hi,
For the design of cryogénic full containment storage tanks, do we have to apply BS EN 14620 all parts along with API 620 or BS EN 14620 alone?
BS EN 14620 part 2 is for metallic components.
Thanks
 
You may look to the other parts of EN 14620;


BS EN 14620 part 1 is for general ,
BS EN 14620 part 2 is for metallic components,
BS EN 14620 part 3 is for concrete components,
BS EN 14620 part 4 is for insulation components,
BS EN 14620 part 5 is for testing, purging, cool down ..

If necessary, a hybrid approach should be considered .( API+ EN 14620 )

I do not understand your position ..
LNG tank business is highly specialized area and some companies have in house standards and details..












Tim was so learned that he could name a
horse in nine languages: so ignorant that he bought a cow to ride on.
(BENJAMIN FRANKLIN )

 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top