I am Hadi and have a quation as follow
We need some LWN flange Astm A 105. We making this flang from forged round bar. And machenical test were down and result in passed astm a 105 machenical requierment, composition test, too. So pls let me to know is have any way to marking them with Astm A 105 and Asme B16.5. If Not, help me wich kind of standard can cover this issue
I am Hadi and have a quation as follow
We need some LWN flange Astm A 105. We making this flang from forged round bar. And machenical test were down and result in passed astm a 105 machenical requierment, composition test, too. So pls let me to know is have any way to marking them with Astm A 105 and Asme B16.5. If Not, help me wich kind of standard can cover this issue