Hi,

Code (ASME IX) mentions that welders shall be qualified by mechanical testing. It also says welders may be qualified by RT.

My doubt is who decides which one to follow?

Regards

AndyVictor
 
Replies continue below

Recommended for you

The manufacturer of the equipment does.

The devil is in the details; she also wears prada.
 
RT is not acceptable for all materials.
 
You also can not RT GMAW welded in short circuit transfer mode.
 