Hi all
while going through a client specification I found that for sour service requirement vessel plate shall have to be Z quality with 35% s.
1.As per nace MR0175 What is the criteria for a service to be declared as Sour?
2.What is this Z quality plate?
3.Vendor is providing me material as SA 516 Gr.70 + HIC . Is it inline with the above requirement?
Please suggest
Thanks in advance
 
Replies continue below

Recommended for you

1. NACE MR0175 defines sour service as any oilfield environment that can cause cracking by mechanisms (SSC and others!) covered in the standard. It is unfortunately not a concise, specific definition. For SSC alone, you can look at Figure 1 which gives the SSC Region (0, 1, 2, 3).

2. Z quality plate appears to reference a test type. See "through thickness properties" about halfway down this page:
3. Maybe. You will need specifics on the intended environment, an understanding of NACE MR0175, and a purchase specification that includes the Z35 requirement.
 