Here is a listing for tension:
This is for pine, not hickory, but it does list tension parallel to the grain:
This one lists many woods, including Hickory, but NOT tensionat all:
You may be able to use the second reference to compare pine to hickory and get a ballpark tensile value for hickory.
This link lists general properties and has some interesting data, but no numbers:
This one states that "Due to difficulties in testing and the limited use for such data, tension parallel to the grain has not been extensively measured and/or reported to date." :
This is for pine, not hickory, but it does list tension parallel to the grain:
This one lists many woods, including Hickory, but NOT tensionat all:
You may be able to use the second reference to compare pine to hickory and get a ballpark tensile value for hickory.
This link lists general properties and has some interesting data, but no numbers:
This one states that "Due to difficulties in testing and the limited use for such data, tension parallel to the grain has not been extensively measured and/or reported to date." :