Hi everybody.

I am working on something that requires a plastic with high gas permeability but can also retain structural integrity with very thin layers. However, I am not familiar with plastics at all so I have no idea where to start. Any tips would be much appreciated :)

 
Replies continue below

Recommended for you

Are you going to make pipe with it?
Just that I don't understand why you posted in this forum.

Only put off until tomorrow what you are willing to die having left undone. - Pablo Picasso
 
It will also help if you define "gas": eg. vinyl is highly permeable to H2S, teflon somewhat pearmeable to HCl,etc.
 