I have run into a problem with manufacturing a part and i am looking for some help to determine what went wrong.
First off we manufactured 2 perfect working parts about 6 months ago. We have now tried to duplicate the process and are having problems. The problem is that the 304SS material is not taking a texture from sandblasting the same as the first time. After the original time sandblasting the parts new parts we found they did not take the required texture we decided to anneal them and try again. We have just received a report saying the parts are still not taking the required texture. I have verified that the sandblasting medium is new and it is the same physical person doing the sandblasting and they are using the same pressure and gun as last time.
We only changed one thing we know of between the first set and this set we are having problems with. The newest set was subcontracted out to a different machine shop. I don't know if this could actually be causing the problem or not. And if it is is there anyway we can fix it.
Any help or suggestions would be much appreciated. Thanks
First off we manufactured 2 perfect working parts about 6 months ago. We have now tried to duplicate the process and are having problems. The problem is that the 304SS material is not taking a texture from sandblasting the same as the first time. After the original time sandblasting the parts new parts we found they did not take the required texture we decided to anneal them and try again. We have just received a report saying the parts are still not taking the required texture. I have verified that the sandblasting medium is new and it is the same physical person doing the sandblasting and they are using the same pressure and gun as last time.
We only changed one thing we know of between the first set and this set we are having problems with. The newest set was subcontracted out to a different machine shop. I don't know if this could actually be causing the problem or not. And if it is is there anyway we can fix it.
Any help or suggestions would be much appreciated. Thanks